« on: March 23, 2009, 04:50:17 PM »
picked up a good condition single drill blueberry,i want to freshen her up after the long journey across the sea...........what in abralon would be her original condition......on the lane 1 site it says gloss polish..........help would be appreciated, thanks
--------------------
black raspberry saw
emerald saw
cranberry c  buzzsaw  
enriched uranium stacked
enriched uranium label
pearl uranium
pearl carbide
pearl cherry bomb
solid cobalt bomb
xxxl starburst
h20 buzzsaw
liberator
solid uranium
clear diamond
bullet buzzsaw
tsunami
uranium hrg
blueberry buzzsaw 14lb
supernova solid
enriched uranium cg out

wanted single drill right hand blueberry 15 lb
wanted single drill right hand silver diamond 15lb

 

SVstar34

  • Hero Member
  • *****
  • Posts: 5464
Re: blueberry saw factory finish
« Reply #1 on: March 24, 2009, 12:51:18 AM »
when in doubt... Ask Beans!
--------------------
My Arsenal:
Rogue Cell (coming soon)
Bounty(4.5 x 4.75 Fresh 1000 Abralon)
Twisted Fury(5 x 4 500 Abralon + Reacta Shine)
Raw Hammer Pain(Leverage 1000 Abralon)
Blue Vibe(5 x 5 4000 Abralon + Reacta Shine)


buzzaussie299

  • Full Member
  • ***
  • Posts: 186
Re: blueberry saw factory finish
« Reply #2 on: March 24, 2009, 02:08:33 AM »
should of thought of that,,lol
--------------------
black raspberry saw
emerald saw
cranberry c  buzzsaw  
enriched uranium stacked
enriched uranium label
pearl uranium
pearl carbide
pearl cherry bomb
solid cobalt bomb
xxxl starburst
h20 buzzsaw
liberator
solid uranium
clear diamond
bullet buzzsaw
tsunami
uranium hrg
blueberry buzzsaw 14lb
supernova solid
enriched uranium cg out

wanted single drill right hand blueberry 15 lb
wanted single drill right hand silver diamond 15lb

beachcomberjones

  • Hero Member
  • *****
  • Posts: 564
Re: blueberry saw factory finish
« Reply #3 on: March 24, 2009, 04:35:47 AM »
try 600 w/ polish
--------------------
Looking for Comet Pro and Solid Viper!!!!

charlest

  • Hero Member
  • *****
  • Posts: 24526
Re: blueberry saw factory finish
« Reply #4 on: March 24, 2009, 06:13:56 AM »
No Abralon was used in finishing those Brunswick made Buzzsaw.
It was probably the standard Brunswick polished finishing process: sand with 400 grit US/CAMI (P800 grit) and use Brunswick High Gloss Factory Finish polish to shine it to a gloss finish.
--------------------
"None are so blind as those who will not see."
"None are so blind as those who will not see."

Buzzhead

  • Hero Member
  • *****
  • Posts: 2002
Re: blueberry saw factory finish
« Reply #5 on: March 24, 2009, 06:18:31 AM »
800 grit with polish.......
hey buzzaussie...... remember me??
LOL.

--------------------
FAILURE IS FEEDBACK. AND FEEDBACK IS THE BREAKFAST OF CHAMPIONS THAT GOT DIGESTED!

Ten pin?????? Where?? I throw a BUZZSAW there is NUTTIN left on the deck...

Proud MEMBER of the FOS!!
Member of the FOS, if there happens to be a 9 pin standing just toss a saw and cut it down~~!
FAILURE IS FEEDBACK. AND FEEDBACK IS THE BREAKFAST OF CHAMPIONS THAT GOT DIGESTED!

Ten pin?????? Where?? I throw a BUZZSAW there is NUTTIN left on the deck...

Proud MEMBER of the FOS!!
Member of the FOS, if there happens to be a 9 pin standing just toss a saw and cut it down~~!

buzzaussie299

  • Full Member
  • ***
  • Posts: 186
Re: blueberry saw factory finish
« Reply #6 on: March 24, 2009, 12:39:03 PM »
of course needed quick answer from someone and when i am awake you guys are asleep lol, dont worry , i will ring you next time i promise lol . When i was cutting her back i think it was 330 am your time lol . Dude this blueberry you sent me is awesome keep em coming , lol
--------------------
black raspberry saw
emerald saw
cranberry c  buzzsaw  
enriched uranium stacked
enriched uranium label
pearl uranium
pearl carbide
pearl cherry bomb
solid cobalt bomb
xxxl starburst
h20 buzzsaw
liberator
solid uranium
clear diamond
bullet buzzsaw
tsunami
uranium hrg
blueberry buzzsaw 14lb
supernova solid
enriched uranium cg out

wanted single drill right hand blueberry 15 lb
wanted single drill right hand silver diamond 15lb

Doug Sterner

  • Hero Member
  • *****
  • Posts: 4395
Re: blueberry saw factory finish
« Reply #7 on: March 27, 2009, 09:57:19 AM »
If I am not mistaken I think Brunswick finished off most of their stuff at 400 grit and then added Rough Buff if you wanted some gloss to it.
--------------------
Doug Sterner
Doug's Pro Shop
Owego, NY

http://dougsproshop@aol.com
www.dougsproshop.net
Lane 1 Buzzsaw...The Official Power Tool Of Bowling
Doug Sterner
Doug's Pro Shop
Owego, NY

Proud Member of the NRA
Fighting to uphold the Constitution of the U.S.