I'm trying to fill the gap between the Solid Uranium and the Tsunami. The Condition I'm fighting is the SU is too much ball and the Tsunami saktes a little too long in the oil. When there is a clean back end the Tsunami is tremendous. I might be getting a little carry down so i wanted something matte and not as strong as the SU.
The SU has pin next to the ring finger and CG stacked. The Tsunami is drilled with the pin under the ring finger and the MB marking directly under the thumb.
I am also drilling another Tsunami with the pin a little below and a little to the right of the ring finger and the MB in a stronger position. Thinking about wet sanding it to 600 and then add a light coat of polish.
Please give me your recommendations.
--------------------
Nicanor (Ten On The Deck)
Edited on 2/23/2006 11:25 PM