i have several of the low flares, the advice i was given from one of the staffers was to drill it stronger than normal as its a pretty weak piece. And it was with the factory OBB surface
Once i dulled it up, it was estimated 3-4 boards stronger
i have used factory finish polish on it with great success, very rolly and continuous, i also bought some of the factory "clean n sheen" polish which a matte finish to replicate the factory OBB
either way, i have used it dull, with polish and with factory clean n sheen polish, all 3 ways produced different results
the numbers on the 2 balls are different, the tag would seem to be over/under if this a little volume because of its high grit surface and polish while the low flare is a different concept. has some underlying surface plus polish and a weaker core